性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 密度 | ASTM D-792 | 0.92 | g/m3 | |
熔體流動(dòng)速率 | 190℃/2.16kg | ISO 1133 | 25 | g/10min | |
物理性能 | 成型收縮率 | ASTM D-955 | 2.4 | % | |
機(jī)械性能 | 環(huán)境開(kāi)裂應(yīng)力 | 50℃, Antarox,Compression Molded | ASTM D-1693 | 6.7 | hr |
環(huán)境開(kāi)裂應(yīng)力 | 50℃, Antarox,Injection Molded | ASTM D-1693 | 1.2 | hr | |
拉伸模量 | Compression Molded | ASTM D-638 | 256 | MPa | |
拉伸模量 | Injection Molded | ASTM D-638 | 155 | MPa | |
拉伸屈服強(qiáng)度 | Compression Molded | ASTM D-638 | 12 | MPa | |
拉伸屈服強(qiáng)度 | Injection Molded | ASTM D-638 | 7.1 | MPa | |
拉伸斷裂強(qiáng)度 | Injection Molded | ASTM D-638 | >11.6 | MPa | |
拉伸斷裂伸長(zhǎng)率 | Injection Molded | ASTM D-638 | > 870 | % | |
IZOD缺口沖擊強(qiáng)度 | -20℃,Injection Molded | ASTM D-256 | No Break | ||
IZOD缺口沖擊強(qiáng)度 | -40℃,Injection Molded | ASTM D-256 | 90 | kJ/m2 | |
IZOD缺口沖擊強(qiáng)度 | 23℃,Injection Molded | ASTM D-256 | No Break | ||
拉伸沖擊強(qiáng)度 | Compression Molded | ISO 8256 | 105 | kJ/m2 | |
邵氏硬度 | Shore D,Compression Molded | ASTM D-2240 | 48 | ||
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 92 | ℃ |